Search Results

There are 66997 results for: content related to: Characterization of Blackglas™/Bn/Nicalon™ Composites

  1. Evaluation of Ammonia Treated Nextel™ 312 Fiber -Blackglas™ Matrix Composites

    Proceedings of the 19th Annual Conference on Composites, Advanced Ceramics, Materials, and Structures - B: Ceramic Engineering and Science Proceedings, Volume 16, Issue 5

    N. R. Khasgiwale, E. P. Butler, K. R. Vaidyanathan, L. Tsakalakos, W. R. Cannon, S. C. Danforth, S.T. Gonczy, Pages: 621–631, 2008

    Published Online : 26 MAR 2008, DOI: 10.1002/9780470314784.ch3

  2. Fabrication and Properties of SiC/SiC Composites Derived from Ceraset™ SN Preceramic Polymer

    Proceedings of the 21st Annual Conference on Composites, Advanced Ceramics, Materials, and Structures: A: Ceramic Engineering and Science Proceedings, Volume 18, Issue 3

    David V. Miller, Donald L. Pommell, Gerhard H. Schiroky, Pages: 409–417, 2008

    Published Online : 26 MAR 2008, DOI: 10.1002/9780470294437.ch46

  3. Tensile Tests of Miniature Fiber Reinforced Ceramic Composites for Screening Process-Property Relations

    Proceedings of the 21st Annual Conference on Composites, Advanced Ceramics, Materials, and Structures: A: Ceramic Engineering and Science Proceedings, Volume 18, Issue 3

    S. T. Gonczy, R. C. Sprandel, K. T. Faber, Pages: 729–736, 2008

    Published Online : 26 MAR 2008, DOI: 10.1002/9780470294437.ch79

  4. Strength and Stability Studies on Mini-Tow Ceramic Composites Made with Nitrided Nextel™ 312 Fibers and Silicon Oxycarbide

    22nd Annual Conference on Composites, Advanced Ceramics, Materials, and Structures: A: Ceramic Engineering and Science Proceedings, Volume 19, Issue 3

    S. T. Gonczy, K. Oba, K. T. Faber, Pages: 147–154, 2008

    Published Online : 26 MAR 2008, DOI: 10.1002/9780470294482.ch17

  5. Blackglas™-Nicalon™ Composites with CVD Boron Nitride Fiber Interface Coatings

    Proceedings of the 19th Annual Conference on Composites, Advanced Ceramics, Materials, and Structures - A: Ceramic Engineering and Science Proceedings, Volume 16, Issue 4

    S. T. Gonczy, E. P. Butler, N. R. Khasgiwale, L. Tsakalakos, W. R. Cannon, S. C. Danforth, Pages: 433–441, 2008

    Published Online : 26 MAR 2008, DOI: 10.1002/9780470314715.ch48

  6. Properties of CVD BN-COATed Hi-Nicalon Fiber Reinforced SiC/SiC Composite

    24th Annual Conference on Composites, Advanced Ceramics, Materials, and Structures: A: Ceramic Engineering and Science Proceedings, Volume 21, Issue 3

    A. Saeki, M. Takeda, A. Yokoyama, T. Yoshida, Pages: 363–370, 2008

    Published Online : 26 MAR 2008, DOI: 10.1002/9780470294628.ch42

  7. Creep and Fatigue Behavior in Hi-Nicalon-Fiber-Reinforced Silicon Carbide Composites at High Temperatures

    Journal of the American Ceramic Society

    Volume 82, Issue 1, January 1999, Pages: 117–128, Shijie Zhu, Mineo Mizuno, Yutaka Kagawa, Jianwu Cao, Yasuo Nagano and Hiroshi Kaya

    Version of Record online : 22 DEC 2004, DOI: 10.1111/j.1151-2916.1999.tb01731.x

  8. Thermal redistribution reactions of Blackglas™ ceramic

    Journal of Applied Polymer Science

    Volume 81, Issue 1, 5 July 2001, Pages: 143–152, Feng Wang, Tom Apple and William N. Gill

    Version of Record online : 18 APR 2001, DOI: 10.1002/app.1424

  9. Tensile Behavior of As-Fabricated and Burner-Rig Exposed SiC/SiC Composites with Hi-Nicalon Type-S Fibers

    26th Annual Conference on Composites, Advanced Ceramics, Materials, and Structures: A: Ceramic Engineering and Science Proceedings, Volume 23, Issue 3

    H. M. Yun, J. A. Dicarlo, L. T. Ogbuji, Y. L. Chen, Pages: 571–580, 2008

    Published Online : 26 MAR 2008, DOI: 10.1002/9780470294741.ch67

  10. Die Rißzähigkeit und Brucharbeit von SiC-faser-verstärkten Glasmatrix-Verbundwerkstoffen: Bestimmung durch die Chevron-Kerb-Technik

    Materialwissenschaft und Werkstofftechnik

    Volume 30, Issue 7, July 1999, Pages: 394–400, A. R. Boccaccini, V. Winkler, M. Reinisch and I. Dlouhy

    Version of Record online : 3 FEB 2000, DOI: 10.1002/(SICI)1521-4052(199907)30:7<394::AID-MAWE394>3.0.CO;2-L

  11. Oxidation kinetics strength of Hi-NicalonTM-S SiC fiber after oxidation in dry and wet air

    Journal of the American Ceramic Society

    Randall S. Hay and Richard J. Chater

    Version of Record online : 8 MAY 2017, DOI: 10.1111/jace.14833

  12. Oxidative Degradation Behavior of Polycarbo-Silane-Derived Silicon Carbide Fibers

    23rd Annual Conference on Composites, Advanced Ceramics, Materials, and Structures : A: Ceramic Engineering and Science Proceedings, Volume 20, Issue 3

    A. Urano, A. Saeki, M. Takeda, A. Yokoyama, Pages: 85–93, 2008

    Published Online : 26 MAR 2008, DOI: 10.1002/9780470294567.ch11

  13. High Temperature Properties and Creep Resistance of Near-Stoichiometric SiC Fibers

    23rd Annual Conference on Composites, Advanced Ceramics, Materials, and Structures: B: Ceramic Engineering and Science Proceedings, Volume 20 Issue 4

    H. Serizawa, C. A. Lewinsohn, G. E. Youngblood, R. H. Jones, D. E. Johnston, A. Kohvama, Pages: 443–450, 2008

    Published Online : 26 MAR 2008, DOI: 10.1002/9780470294574.ch52

  14. High Performance Silicon Carbide Fiber Hi-Nicalon for Ceramic Matrix Composites

    Proceedings of the 19th Annual Conference on Composites, Advanced Ceramics, Materials, and Structures - A: Ceramic Engineering and Science Proceedings, Volume 16, Issue 4

    M. Takeda, J. Sakamoto, A. Saeki, Y. Imai, H. Ichikawa, Pages: 37–44, 2008

    Published Online : 26 MAR 2008, DOI: 10.1002/9780470314715.ch3

  15. Thermal Stability of Polycarbosilane-Derived Silicon Carbide Fibers under Reduced Pressures

    Journal of the American Ceramic Society

    Volume 84, Issue 3, March 2001, Pages: 566–570, Toshio Shimoo, Hiroshi Takeuchi and Kiyohito Okamura

    Version of Record online : 20 DEC 2004, DOI: 10.1111/j.1151-2916.2001.tb00699.x

  16. Influence of Interface Characteristics on the Mechanical Properties of Hi-Nicalon type-S or Tyranno-SA3 Fiber-Reinforced SiC/SiC Minicomposites

    International Journal of Applied Ceramic Technology

    Volume 7, Issue 3, May/June 2010, Pages: 291–303, C. Sauder, A. Brusson and J. Lamon

    Version of Record online : 16 FEB 2010, DOI: 10.1111/j.1744-7402.2010.02485.x

  17. Effect of High-Temperature Loading on Mechanical Properties of Nicalon Fibers and Nicalon Fiber/SiC Matrix Composites

    Proceedings of the 17th Annual Conference on Composites and Advanced Ceramic Materials, Part 2 of 2: Ceramic Engineering and Science Proceedings, Volume 14, Issue 9/10

    Dileep Singh, Jitendra P. Singh, Pages: 1153–1164, 2008

    Published Online : 26 MAR 2008, DOI: 10.1002/9780470314234.ch54

  18. Hot Corrosion of Two Nicalon Fiber Reinforced Glass-Ceramic Matrix Composites

    Proceedings of the 17th Annual Conference on Composites and Advanced Ceramic Materials, Part 1 of 2: Ceramic Engineering and Science Proceedings, Volume 14, Issue 7/8

    S.-W. Wang, R. W. Kowalik, R. Sands, Pages: 385–398, 2008

    Published Online : 28 MAR 2008, DOI: 10.1002/9780470314180.ch63

  19. Evaluation of the Interfacial Mechanical Properties of Fiber Reinforced Boron Nitride Matrix Composites

    Proceedings of the 18th Annual Conference on Composites and Advanced Ceramic Materials - A: Ceramic Engineering and Science Proceedings, Volume 15, Issue 4

    C. G. Cofer, J. Economy, M. K. Ferber, E. Lara-Curzio, Pages: 446–455, 2008

    Published Online : 28 MAR 2008, DOI: 10.1002/9780470314500.ch50

  20. Measurement of Gas Transport through Fiber Preforms and Densified Composites for Chemical Vapor Infiltration

    Journal of the American Ceramic Society

    Volume 81, Issue 5, May 1998, Pages: 1298–1304, Thomas L. Starr and Nicole Hablutzel

    Version of Record online : 20 JAN 2005, DOI: 10.1111/j.1151-2916.1998.tb02481.x