Delayed Failure of Silicon Carbide Fibres in Static Fatigue at Intermediate Temperatures (500-800°C) in Air

  1. Edgar Lara-Curzio,
  2. Jonathan Salem and
  3. Dongming Zhu
  1. W. Gauthier and
  2. J. Lamon

Published Online: 14 DEC 2009

DOI: 10.1002/9780470339497.ch41

Mechanical Properties and Performance of Engineering Ceramics and Composites III

Mechanical Properties and Performance of Engineering Ceramics and Composites III

How to Cite

Gauthier, W. and Lamon, J. (2007) Delayed Failure of Silicon Carbide Fibres in Static Fatigue at Intermediate Temperatures (500-800°C) in Air, in Mechanical Properties and Performance of Engineering Ceramics and Composites III (eds E. Lara-Curzio, J. Salem and D. Zhu), John Wiley & Sons, Inc., Hoboken, NJ, USA. doi: 10.1002/9780470339497.ch41

Publication History

  1. Published Online: 14 DEC 2009
  2. Published Print: 29 OCT 2007

ISBN Information

Print ISBN: 9780470196335

Online ISBN: 9780470339497

SEARCH

Keywords:

  • silicon carbide fibres;
  • static fatigue;
  • delayed failure;
  • crack growth;
  • ceramic matrix composites

Summary

This chapter contains sections titled:

  • Introduction

  • Experimental Procedure

  • Results and Discussion

  • Conclusions