Durability of cathodes including Cr poisoning

Advances in Electrocatalysis, Materials, Diagnostics and Durability

Materials for high temperature fuel cells

Materials durability

  1. N. H. Menzler,
  2. A. Mai,
  3. D. Stöver

Published Online: 15 DEC 2010

DOI: 10.1002/9780470974001.f500038

Handbook of Fuel Cells

Handbook of Fuel Cells

How to Cite

Menzler, N. H., Mai, A. and Stöver, D. 2010. Durability of cathodes including Cr poisoning. Handbook of Fuel Cells. .

Author Information

  1. Institute of Energy Research, Jülich, Germany

Publication History

  1. Published Online: 15 DEC 2010

Options for accessing this content:

  • If you are a society or association member and require assistance with obtaining online access instructions please contact our Journal Customer Services team.
    http://wiley.force.com/Interface/ContactJournalCustomerServices_V2.
  • Login via other institutional login options http://onlinelibrary.wiley.com/login-options.
  • You can purchase online access to this Article for a 24-hour period (price varies by title)
    • If you already have a Wiley Online Library or Wiley InterScience user account: login above and proceed to purchase the article.
    • New Users: Please register, then proceed to purchase the article.

Login via OpenAthens

or

Search for your institution's name below to login via Shibboleth.

Please register to:

  • Save publications, articles and searches
  • Get email alerts
  • Get all the benefits mentioned below!

Register now >