Kinetics of Passive Oxidation of Hi-Nicalon-S SiC Fibers in Wet Air: Relationships between SiO2 Scale Thickness, Crystallization, and Fiber Strength

  1. Dileep Singh,
  2. Jonathan Salem,
  3. Michael Halbig and
  4. Sanjay Mathur
  1. R. S. Hay1,
  2. G. E. Fair1,
  3. A. Hart2,
  4. S. Potticary2 and
  5. R. Bouffioux3

Published Online: 6 DEC 2012

DOI: 10.1002/9781118217467.ch24

Mechanical Properties and Performance of Engineering Ceramics and Composites VII

Mechanical Properties and Performance of Engineering Ceramics and Composites VII

How to Cite

Hay, R. S., Fair, G. E., Hart, A., Potticary, S. and Bouffioux, R. (2012) Kinetics of Passive Oxidation of Hi-Nicalon-S SiC Fibers in Wet Air: Relationships between SiO2 Scale Thickness, Crystallization, and Fiber Strength, in Mechanical Properties and Performance of Engineering Ceramics and Composites VII (eds D. Singh, J. Salem, M. Halbig and S. Mathur), John Wiley & Sons, Inc., Hoboken, NJ, USA. doi: 10.1002/9781118217467.ch24

Author Information

  1. 1

    Air Force Research Laboratory, Materials and Manufacturing Directorate, WPAFB, OH

  2. 2

    U. Cincinnati, Cincinnati, OH

  3. 3

    New Mexico Tech. U., Socorro, NM

Publication History

  1. Published Online: 6 DEC 2012
  2. Published Print: 19 NOV 2012

ISBN Information

Print ISBN: 9781118205884

Online ISBN: 9781118217467

SEARCH

Keywords:

  • passive oxidation;
  • crystallization;
  • fiber strength;
  • strength degradation;
  • activation energy

Summary

This chapter contains sections titled:

  • Introduction

  • Experiments

  • Results and Discussion