Evaluating the Effect of Pre-Ageing Deformation on β' Precipitate Size and Distribution in Mg-Zn(-Y) Alloys

  1. Suveen N. Mathaudhu,
  2. Wim H. Sillekens,
  3. Neale R. Neelameggham and
  4. Norbert Hort
  1. Julian M Rosalie1,
  2. Hidetoshi Somekawa1,
  3. Alok Singh1 and
  4. Toshiji Mukai2

Published Online: 15 MAY 2012

DOI: 10.1002/9781118359228.ch36

Magnesium Technology 2012

Magnesium Technology 2012

How to Cite

Rosalie, J. M., Somekawa, H., Singh, A. and Mukai, T. (2012) Evaluating the Effect of Pre-Ageing Deformation on β' Precipitate Size and Distribution in Mg-Zn(-Y) Alloys, in Magnesium Technology 2012 (eds S. N. Mathaudhu, W. H. Sillekens, N. R. Neelameggham and N. Hort), John Wiley & Sons, Inc., Hoboken, NJ, USA. doi: 10.1002/9781118359228.ch36

Author Information

  1. 1

    Microstructure Design Group, National Institute for Materials Science (NIMS), Sengen 1-2-1, Tsukuba, Ibaraki, 305-0047, Japan.

  2. 2

    Dept. Mechanical Engineering, Kobe University, 1-1 Rokkodai, Nada, Kobe city, 657-8501 Japan

Publication History

  1. Published Online: 15 MAY 2012
  2. Published Print: 17 MAR 2012

ISBN Information

Print ISBN: 9781118291214

Online ISBN: 9781118359228

SEARCH

Keywords:

  • Magnesium alloys;
  • Precipitation

Summary

This chapter contains sections titled:

  • Introduction

  • Experimental

  • Results

  • Discussion