Production of Potassium Titanate Whisker Reinforced Dental Composites

  1. Roger Narayan,
  2. Paolo Colombo,
  3. Soshu Kirihara and
  4. Sujanto Widjaja
  1. Derya Kapusuz1,
  2. Jongee Park2 and
  3. Abdullah Ozturk1

Published Online: 22 NOV 2013

DOI: 10.1002/9781118807811.ch3

Advances in Bioceramics and Porous Ceramics VI

Advances in Bioceramics and Porous Ceramics VI

How to Cite

Kapusuz, D., Park, J. and Ozturk, A. (2013) Production of Potassium Titanate Whisker Reinforced Dental Composites, in Advances in Bioceramics and Porous Ceramics VI (eds R. Narayan, P. Colombo, S. Kirihara and S. Widjaja), John Wiley & Sons, Inc., Hoboken, NJ, USA. doi: 10.1002/9781118807811.ch3

Author Information

  1. 1

    Metallurgical and Materials Engineering, Middle East Technical University, Ankara, Turkey

  2. 2

    Metallurgical and Materials Engineering, Atilim University, Ankara, Turkey

Publication History

  1. Published Online: 22 NOV 2013
  2. Published Print: 21 OCT 2013

ISBN Information

Print ISBN: 9781118807668

Online ISBN: 9781118807811

SEARCH

Keywords:

  • potassium titanate whiskers;
  • reinforced dental composites;
  • photocatalytic activity;
  • methylene blue degradation test;
  • molar compositions

Summary

This chapter contains sections titled:

  • Introduction

  • Experimental

  • Production of KTW

  • Production of Reinforced and Unreinforced Udma-Tegdma Resins

  • Characterization and Testing

  • Results

  • XRD Analysis

  • HR-TEM Analysis

  • Bet Analysis

  • Wear and Nano-Indentation Testing of Unreinforced Resin Mixtures and KTW Reinforced Resin Composites

  • Methylene Blue (MB) Degradation of the KTW, Unreinforced Resin Mixtures and KTW Reinforced Resin Composites

  • Discussion

  • Conclusion

  • Acknowledgement