Axial pressure profiles in non-newtonian flow: Part II: Viscometric flow and relaxation phenomena analyses

Authors


  • This paper was presented in part at the 21st Canadian Chemical Engineering Conference, October 12-15, 1971, Montreal, Quebec.

Abstract

Extensive pressure profile data were compiled for a 16.5% polyisobutylene solution in mineral spirits. Values of stored elastic energy obtained from these data compare favorably with those ascertained from die swell and from entrance correction methods. The viscometric normal stress differences were significantly larger than the shear stress and, particularly, the second normal stress rose to a maximum where it was an order of magnitude larger than the first normal stress difference. Time constants calculated from swell decay and entrance-borne elastic stress relaxation are essentially the same and show an approximate inverse relation to the shear rate.

Abstract

On a assemblé des données élaborées sur des profils de presion, dans le cas d'une solution (de 16.5% de concentration) de polyisobutyléne dans un solvant de pétrole. Les valeurs d'énergie élastique emmagasinées qu'ou a obtenues à partir des dites données se sont comparées avantageusement avec celles qu'on avait notées avec le gonflement du moule et les méthodes de correction à l'entrée. Les différences en viscosité de la contrainte normale se sont avérées appréciablement plus grandes que dam le cas de la contrainte de cisaillement; en outre, la seconde contrainte normale a atteint un sommet qui correspondait à un ordre de grandeur plus élevé que la différence de la premiire coutrainte normale. On a trouvé que les constantes de temps, calculées à partir de la diminution du gonflement et de la relaxation de la contrainte élastique produite à l'entrée, étaient essentiellement les mêmes et étaient en relation approximativement inverse à la vitesse de cisaillement.

Ancillary