Oxidation of low concentrations of hydrogen sulfide over activated carbon

Authors


Abstract

The oxidation of low concentrations of hydrogen sulfide with air over activated carbon was studied over the temperature range 24-200°C using both fixed and fluid bed reactors. The predominant reaction, H2S + ½ Oa → H2O + S, was found to have an order of 0.5 with respect of H2S concentration. Activity of the catalyst decreased as the amount of sulfur deposited on it increased. Indirect evidence suggests that adsorption of water by the carbon also decreases its activity as a catalyst at lower temperatures. Values of the activation energy and the frequency factor were determined for various sulfur loadings using the fixed bed reaction system. Regeneration of the carbon loaded with sulfur was studied at temperatures between 150 and 500°C using steam as a carrier gas. Bright yellow sulfur was recovered. The regenerated carbon was shown to have its original activity.

Abstract

On a étudié, sur une gamine de température de 24 à 200°C et en employant des réacteurs à lit fixe et à lit fluide, l'oxydation par l'air de l'hydrogène sulfuré en faibles concentrations, sur du carbone activé. On a trouvé que la réaction prédominante H2S + ½O2 → H2 + S avait un ordre de 0.5 par rapport à la concentration de H2S. L'activité du catalyseur a diminué à mesure que la quantité de soufre déposé s'accroissait. II appert indirectement que l'adsorption d'eau par le carbone diminue aussi son activité comme catalyseur à des températures moindres. On a déterminé les valeurs de l'énergie d'activation et du facteur de fréquence, pour diverses charges de soufre, en employant le système de réacteur à lit fixe. On a étudié la régénération du carbone recouvert de soufre en employant de la vapeur d'eau comme gaz porteur, à des températures comprises entre 150 et 500°C. On a récupéré du soufre de couleur jaune vif; on a constaté que le carbone régénéré possédait son activité catalytique initiale.

Ancillary