Liquefaction of aspen poplar wood

Authors


  • Presented in part at the Canadian Chemical Conferences: Vancouver, June 1979; Ottawa, June 1980; Halifax, June 1981.

Abstract

Dried and green aspen poplar wood suspended in water containing alkaline catalysts has been converted completely to an oil, water-soluble chemicals and gases if heated for one hour in the presence of carbon monoxide in a rocking batch reactor. Within the ranges of parameters studied: temperature (593—633 K), nominal reaction times (0—1 h), water-to-wood ratio (0.5:1—5:1), catalyst (Na2CO3, K2CO3, NaOH), amount of catalyst (7.0—12.5 wt %) and initial hydrogen to carbon monoxide ratios (2:1—0:1), the water-to-wood ratio was most important. Oil yields of ˜50% with a carbon plus hydrogen content of ˜80% and representing a carbon recovery of ˜66% were obtained. The higher heats of combustion ranged from 32.2 to 36.0 MJ/kg.

Abstract

Du bois de peuplier faux tremble (vert ou séché), en suspension dans l'eau contenant des catalyseurs alcalins est totalement converti en huile, en produits solubles dans l'eau et en gaz, lorsqu'on le chauffe pendant une heure en présence de monoxyde de carbone dans un réacteur discontinu à bascule. Sur les gammes des paramètres étudiées: (a) température (593—633 K), (b) durée nominale de réaction (0—1 heure), (c) rapport eau/bois (0.5: 1—5: 1), (d) catalyseur (Na2CO3, K2CO3, NaOH), (e) quantité de catalyseur (7.0 à 12.5% en poids) et (f) rapport initial hydrogène/monoxyde de carbone (2: 1, 0: 1), la valeur du rapport eau/bois s'est avérée très importante. On a obtenu des rendements en huile de ˜50% avec des teneurs de ˜80% en carbone et hydrogène, ce qui représente une récupération de carbone de ˜66%. Les chaleurs de combustion les plus élevées ont varié 32.2 et 36.0 MJ/kg.

Ancillary