Authors


Abstract

Poplar wood, when heated rapidly (70-90 s) in water to 350°C and quenched, yields oil in 55 per cent mass yield. Approximately 75 per cent of the wood carbon and hydrogen is retained in the oil. The oil contains 25 per cent oxygen (wood contains 45 per cent). Extended reaction significantly lowers yields which are the same in the presence of both nitrogen and hydrogen atomsopheres. Nickel carbonate addition lowers yields significantly. Experiments have been limited to wood particles less than 35 mesh (0.73 mm grid) but heat transfer studies are being extended to larger particles.

Abstract

On a chauffé rapidement (70 à 90 s) du bois de peuplier dans l'eau à 350°C et on l'a ensuite refroidit brusquement; on a ainsi obtenu une huile avec un rendement en masse de 55%. Environ 75% du carbone et de l'hydrogène du bois ont été retenus dans l'huile qui contient 25% d'oxygène (le bois en contient 45%). Une augmentation du temps de réaction abaisse d'une manière importante les rendements et ceux-ci sont les měmes en présence d'atmosphères d'azote ou d'hydrogène. L'addition de carbonate de nickel a abaissé les rendements d'une manière significative. Les expériences ont été limitées à des particules de dimensions inférieures à 35 mesh (tamis de 0.73 mm), mais les études actuelles portent sur le transfert de la chaleur à des particules de plus grandes dimensions.

Ancillary