Keywords:

  • Populus deltoides;
  • enzymatic saccharification;
  • thermo-mechanical pretreatment;
  • wood slurry hydrothermolysis

Abstract

Ground Populus deltoides was pretreated using a thermo-mechanical process in which shear forces are applied by rapid passage of concentrated slurries (10-14%) through homogenizing valves. The process permits accurate control of operational parameters to induce varying degrees of ultrastructure modification in the substrate. The poplar was pretreated at two levels of severity in the absence of mineral acid and a process time of the order of 2 minutes. The high severity pretreated substrate was more susceptible than commercial α-cellulose to enzymatic saccharification by T. reesei cellulase supplemented with cellobiase (glucose yields of 103 ± 6% and 76.2 ± 1.8% respectively in 48 hours).

On a prétraité du Populus deltoides par un procédé thermomécanique dans lequel on applique des forces de cisaillement en effectuant un passage rapide de suspensions concentrées (10-14%) au travers de vannes homogénéisantes. Ce procédé permet de contrôler de manière précise les paramètres de fonctionnement en permettant d'induire divers degrés de modification de l'ultrastructure dans le substrat. Le peuplier a été traité a deux niveaux de sévérité en l'absence d'acide minèral pendant un temps de traitement de l'ordre de deux minutes. Le substrat prétraité à un niveau de sévérité élevé répond mieux à une saccharification enzymatique par la cellulase T. reesei combinée à de la cellobiase que la alpha-cellulose commerciale (rendement en glucose de 103 ± 6% et 76.2 ± 1.8% en 48 heures respectivement).