Abstract

CentaurTM carbon (Calgon Carbon Corp.) was used as a catalyst for SO2 oxidation in a trickle bed under periodic interruption of its liquid flow for cycle periods from 15 to 60 min, cycle splits (split being the proportion of a cycle in which liquid flows) from 0.0083 to 0.2, and feed temperatures about 80°C.

SO2 removal in the trickle bed was improved at longer periods. At a fixed period of 15 min, a maximum occurred with split. At high splits, platinized and unplatinized carbons performed indistinguishably. Results suggested kinetic rate control at low splits and oxygen mass transport control at high splits.

On a utilisé du carbone CentaurTM (Calgon Carbon Corp.) comme catalyseur pour l'oxydation du SO2 dans un lit ruisselant avec interruption périodique de l'écoulement liquide pour des périodes de circulation allant de 15 à 60 minutes, des fractions de cycle comprises entre 0,0083 et 0,2 (la fraction étant la proportion d'un cycle durant laquelle s'écoule le liquide) et des températures d'alimentation d'environ 80°C.

Le retrait du SO2 dans le lit ruisselant est amélioré pour les fractions les plus longues. Á une période fixe de 15 minutes, le retrait atteint un maximum. À des fractions élevées, les carbones platinisés et non platinisés ont donné les měmes performances. Les résultats suggèrent que la cinétique contrǒle pour les petites fractions tandis que le transfert d'oxygène contrǒle aux fractions élevées.