Phenolic compounds from vacuum pyrolysis of wood wastes

Authors


Abstract

Various softwood and hardwood bark residues, primary sludges and softwood sawdust residues were processed by vacuum pyrolysis in a laboratory scale batch reactor. The pyrolysis oil, water, charcoal, and gas were recovered and analyzed. The pyrolysis oils were analyzed in details for their content in phenolic compounds after derivatization to their acetyl derivatives. The influence of temperature, heating rate, feedstock bed thickness, particle size and feedstock water pretreatment on the yield of phenols was investigated. The highest yield of phenols was obtained when hardwood bark was soaked in water for 48 hours and pyrolyzed at a temperature of 450°C and a heating rate of 10°C/min. Pyrolysis performance was evaluated in terms of total phenolic yield and composition.

Abstract

Divers résidus d'écorce de bois dur et de bois tendre, des boues primaires et des résidus de sciure de bois tendre ont été traités par pyrolyse sous vide dans un réacteur continu à l'échelle de laboratoire. L'huile, l'eau, le charbon de bois et le gaz de pyrolyse ont été récupérés et analysés. Les huiles de pyrolyse ont été analysées en détail pour déterminer leur teneur en composés phénoliques après transformation en leur dérivés acétyliques. On a étudié l'influence de la température, de la vitesse de chauffe, de l'épaisseur du lit de matière première, de la taille des particules et du prétraitement de l'eau d'alimentation sur le rendement en phénol. Le rendement en phénol le plus élevé a été obtenu lorsque l'écorce de bois dur a été trempée dans l'eau pendant 48 heures et pyrolysée à une température de 450°C, avec une vitesse de chauffe de 10°C/min. On a évalué la performance de la pyrolyse quant au rendement total et à la composition des phénols.

Ancillary