A study of the polymerization of styrene initiated by various tetralkyl thiuram disulfides has been made at the temperature range from 50 to 90°C. It was proved that the rate of polymerization increased with the 0.3–0.5 power of the Concentration of thiuram initiator and showed an over-all activation energy of 17 to 23 Kcal./mole. These thiuram disulfides had a retarding action on the polymerization of styrene and weak initiating Activity under thermal conditions. However; in the presence of Eght, they were excellent as polymerization initiators.

Abstract

Die Polymerisation von Styrol bei Zugabe verschiedener Tetralkylthiuram-disulfide wurde bel 50–90°C. untersucht. Es wurde gefunden, daß die Polymerisationsgeschwindigkeit mit der 0,3–0,5 ten Potenz der Thiurarm-Initiatorkonzentration zunahm, und es ergab sich eine totale Aktivationsenergie von 17–23 kcal/Mol. Thiuram-disulfide zeigen eine verzögernde Wirkung bei der Polymerisation des Styrols und eine schwache Initiatorwirkung unter thermischen Bedingungen. In Gegenwart von Licht sind sie sehr gute Polymerisationsinitiatoren.

Ancillary