Nathalie Limodin, Julien Réthoré, Jean-Yves Buffière, François Hild, Wolfgang Ludwig, Johann Rannou and Stéphane Roux 3D X-ray Microtomography Volume Correlation to Study Fatigue Crack Growth Advanced Engineering Materials 13

Version of Record online: 12 NOV 2010 | DOI: 10.1002/adem.201000235

Thumbnail image of graphical abstract

Global DVC is used to analyze a series of computed tomography images of a nodular graphite cast iron specimen subjected in situ to a fatigue test. DVC provides 3D displacement fields in the bulk, crack geometry from residuals (Figure 1) and, finally SIFs all along the crack front.